Effects of high silicon contents on graphite morphology and room temperature mechanical properties of as-cast ferritic ductile cast irons. Part II – Mechanical properties

In this second part of the investigation, room temperature mechanical properties and hardness evolution of cast irons with silicon contents ranging from 2.29 wt% to 9.12 wt% have been studied and related to structural results from the first part. Increasing silicon content increases ultimate tensile strength and yield stress until a maximum value of 719 MPa at around 5.0−5.2 wt% silicon for the former and 628 MPa at 5.2−5.4 wt% silicon for the latter. Brinell hardness remains increasing with silicon content with a maximum value of 396 at 9.12 wt% silicon. Elongation at rupture shows an opposite evolution and gradually decreases to zero at 5.3 wt% silicon. This evolution is related to chemical ordering of the ferritic matrix (embrittlement effect). Chunky graphite shows apparently no significant effect on the ultimate tensile strength and yield strength in cast irons with silicon contents higher than 4.0 wt%. However, it has a negative effect on elongation. This result contrasts with the negative effect of chunky graphite on mechanical properties of ductile irons reported in the literature for alloys with silicon contents lower than 3 wt%. It is suggested that this difference is due to the matrix strengthening effect of high silicon contents which overtakes the detrimental effect of chunky graphite. This study suggests that cast irons with silicon content as high as 5.0 wt% could be considered for industrial applications when high resistance and some ductility are requested.

Autoreak:

Rodolfo González-Martínez, Urko de la Torre, André Ebel (CIRIMAT), Jacques Lacaze (CIRIMAT), Jon Sertucha

Keyword-ak:

Alto silicio, fundición de hierro, fundición dúctil, propiedades mecánicas, grafito chunky. 

Atzera

Nola lagun diezazukegu?

Manten zaitez AZTERLANeko informazioez eguneratuta

Jarri kontaktuan Andoni-rekin

Contacta con Ramón

Jarri kontaktuan Xabierrekin

Jarri kontaktuan Maider Muro-rekin.

Jarri kontaktuan Dr. Urko de la Torre-rekin.

Contacta con Dra. Anna Regordosa

Jarri kontaktuan Aitor Loizaga-ekin.

Jarri kontaktuan Dr. Rodolfo González-Martínez-ekin.

Jarri kontaktuan Anderrekin.

Jarri kontaktuan David Aristondo-rekin.

Jarri kontaktuan Juan J. Bravo-rekin.

Jarri kontaktuan David Garcia-rekin.

Jarri kontaktuan Jose Ramon-rekin.

Jarri kontaktuan Oihana-rekin.

Mantendu AZTERLANeko berrien adi

Jarri kontaktuan David-ekin.

Jarri kontaktuan Ibonekin.

Jarri kontaktuan Hegoirekin.

Jarri kontaktuan Itziarrekin.

Jarri kontaktuan Erikarekin.

Jarri kontaktuan Beñatekin.

Jarri kontaktuan John-ekin

Jarri kontaktuan José Javier-ekin.

Jarri kontaktuan Andrearekin.

Jarri kontaktuan Janirerekin.

Jarri kontaktuan Clararekin.

Jarri kontaktuan Nagorerekin

Jarri kontaktuan Gorkarekin.

Jarri kontaktuan Emilirekin.

Jarri kontaktuan Jonekin.

Metalurgiaren eta metalen eraldatze prozesuen alor desberdinetan lantaldeak sortzen ditugu

Ezagutza alora
Emaiguzu informazio gehiago zure lantaldearen ezagutza beharrei buruz zure helburuetara egokitutako proposamen bat egin ahal izateko.
KONTAKTURAKO DATUAK

Emaizkiguzu zure lanaren datuak eta zurekin kontaktuan jarriko gara ahalik eta bizkorren.

Zein da zure erronka?

Partekatu zure erronka gure lantaldearekin. Hitz egiteak irtenbide posibleetara hurbildu baino ezin gaitzake egin.