Studying a series of near eutectic spheroidal graphite cast irons with various amounts of silicon up to 9.12 wt% confirmed that: 1. silicon stabilizes ferrite to such an extent that ferrite is the Fe-rich phase appearing during solidification at the highest silicon contents; 2. silicon triggers graphite degeneracy such as chunky graphite. As well-known, cerium and magnesium do also increase the risk of chunky graphite formation while antimony counteracts cerium. Based on the metallographic observations of the present work, an index is proposed to evaluate the risk of chunky graphite appearance from the silicon, magnesium, cerium and antimony contents. Above a critical value of this index, the risk for chunky graphite formation increases steadily. Using data from previous studies, it is further demonstrated that the critical value decreases with increase in casting modulus as expected. The evolution of mechanical properties of the prepared cast irons will be presented in a second part of this study.
Rodolfo González-Martínez (AZTERLAN), Urko de la Torre (AZTERLAN), Jacques Lacaze (CIRIMAT, Université de Toulouse), Jon Sertucha (AZTERLAN)
high silicon, dutile iron, mechanical properties, chunky graphite.
How can we help you?
Mantente informad@ de la actividad de AZTERLAN.
Keep up with AZTERLAN’s activity.
Keep up with AZTERLAN’s activity.
We train workforce in different fields regarding the production of metallic alloys, components and structures.
We will contact you as soon as possible.
Share your challenge with us.